ASTM A182 F22 is a low alloy steel predominately used in wellhead applications as an upgrade over AISI 4130. It is a very deep hardening, heat treatable alloy steel.
TM Steels can provide all materials produced to bespoke customer requirements. We project manage your raw material or semi finished material requirements, including Sawing, Heat Treatment, Testing, Rough Machining, Hardness Testing, Ultrasonic Examination and certification, including BS EN 10204 3.1 & BS EN 10204 3.1 Witness documentation packages. We use an approved list of European Mills, and can offer material with PED / REACH & ROHS approval & UKAS accredited Testing. Contact our sales team today if you would like to enquire about our A182F22 Stock Lines.
|
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Ni |
Al |
Cu |
Sn |
|
Min |
0.10 |
0.15 |
0.30 |
|
|
2.0 |
0.87 |
|
|
||
|
Max |
0.15 |
0.50 |
0.60 |
0.015 |
0.025 |
2.50 |
1.13 |
0.50 |
0.05 |
0.25 |
0.10 |
|
Annealed - suitable for further heat treatment to below requirements. |
|||||
|
80 KSI Min |
105 KSI Min |
ASTM A182 Class 3 |
|||
|
UTS |
100 KSI Min |
UTS |
120 KSI Min |
UTS |
75 KSI Min |
|
0.2% Proof Stress |
80 KSI Min |
0.2% Proof Stress |
105 KSI Min |
0.2% Proof Stress |
45 KSI Min |
|
Elongation |
18.00% |
Elongation |
18.00% |
Elongation |
20.00% |
|
Red of Area |
35.00% |
Red of Area |
35.00% |
Red of Area |
30.00% |
|
Hardness |
217/237 |
Hardness |
262/321 |
Hardness |
156/207 |
SURFACE CONDITION
Peeled/smooth turned bar.
REDUCTION RATIO
4:1 Min
STRUCTURE
Grain size will be ASTM 5 or finer.
ULTRASONIC EXAMINATION
Ultrasonic examination available per ASTM A388/API6A Latest Edition or to bespoke customer specification.
Rolled / Peeled Bar
Suitable for heat treatment.
76.2mm – 230mm ⌀
Forged Annealed Bar
Suitable for heat treatment.
254mm – 609.6mm ⌀
DIN 1.7380 10CrMo9-10 ASTM A182 F22